| T O P I C R E V I E W |
| HappyChef |
Posted - 20 Apr 2013 : 09:20:51 Hi guys Ime going to antifoul my Norman 23, just wondered if anyone could advise me of roughly how many litres for 2 coats.
Thanks John.
www.Queensheadaskham.com FB:Queens Head Askham |
| 3 L A T E S T R E P L I E S (Newest First) |
| HappyChef |
Posted - 21 Apr 2013 : 14:07:03 Thanks guy's.
John
www.Queensheadaskham.com FB:Queens Head Askham |
| kev13 |
Posted - 20 Apr 2013 : 20:47:46 I've done my 23 with 3 coats and got paint left from 5 ltrs |
| df |
Posted - 20 Apr 2013 : 09:52:17 A 2.5 litre tin should do you, start at the waterline and work down then second coat do the same, if you run out half way through at least the waterline looks pretty, you don't get that much growth underneath on inland water, leave an inch gap around outdrive/outboard as anti-foul often encourages galvanic corrosion if electrically conected to aluminium.

NBAS--The communal colostomy bag of the boating community. Visit leomagill.co.uk |